Standard for Welding Procedure and Performance Qualification9780871712356, 0871712350

Author : American Welding Society
Description:This specification provides the requirements for qualification of welding procedure specifications, welders, and welding operators for manual, semiautomatic, mechanized, and automatic welding. The welding processes included are oxyfuel gas welding, shielded metal arc welding, gas tungsten arc welding, submerged arc welding, gas metal arc welding, flux cored arc welding, plasma arc welding, electroslag welding, electrogas welding, electron beam welding, laser beam welding, and stud arc welding. Base metals, filler metals, qualification variables, and testing requirements arc also included.
Categories: Technology industrial equipment and technology
Year :1984
Publisher : American Welding Society
Language : English
N° Of Pages : 221